The vial was then submerged in hexanes to swell the PDMS membrane at which point it delaminated from the glass vial. The PDMS thimbles were dried and used as is. Fabrication of cyclooctene:dicyclopentadiene thimbles: Cyclooctene (10 mL, 8.46 g, 779.86