A 5.0% w/w dispersion of PSMA 32 –PTFEMA 53 nanoparticles in n-dodecane (4.5 mL) was added to a 14 mL glass vial. This was then homogenized with various aqueous solutions (prepared with deionized water at around pH 6, unless stated otherwise) (0.5 mL; containing 0–0.43 M NaCl) for 2 min at 20 °C by using an IKA Ultra-Turrax T-18 homogenizer equipped with a 10 mm dispersing tool and